Heat sink specification: fin geometry, flatness and the interface
A heat sink is judged on one number – the thermal resistance it achieves with your interface material at your airflow. Everything on the drawing should protect that number.
Picking the process from the geometry
| Process | Best for | Limits | Tooling |
|---|---|---|---|
| Extruded + cut | Long straight fins, constant cross-section | Fin ratio limited by the die; no cross-cut fins | Die cost amortised over volume |
| Bonded fins | High fin density, wide bases, cross-cut | Thermal path through the bond line | Low – fins are stock |
| Skived | Thin dense fins from a solid block | Base thickness must support the cut | Machine setup only |
| Machined | Small parts, pockets, mounting features | Cost rises fast with fin count | None |
| Die cast | Complex shapes with bosses and ribs | Lower conductivity than wrought; draft angles | Die cost |
The interface face is the part that matters
- Flatness: 0.05 mm across the contact area is the standard; 0.02 mm where the gap pad is thin
- Roughness: Ra 0.8 – 1.6 µm – too smooth and the paste does not wet out, too rough and the bond line thickens
- No anodising on the contact face: anodise is an insulator. Mask it or machine after coating
- Mark the contact area on the drawing so it survives the process route
Fin geometry that a machine can actually cut
- Fin thickness: 0.8 – 1.5 mm skived, 1.0 – 2.0 mm extruded, 1.5 mm and up machined
- Fin pitch: at least 1.5 x fin thickness plus chip clearance for machining
- Fin height to thickness ratio: keep under 15:1 for machined fins, 20:1 for skived
- Base thickness: at least 2 mm under the fin root, more where a thread is cut
Mounting and flatness fight each other
A screw that pulls the base down to a non-flat chassis bends the heat sink and opens the interface on the other side. Two practical fixes: mount through slotted holes so the sink is not pre-loaded, or use a spring clip with a defined force. Where the sink is bolted hard, specify the flatness after assembly, not before.
The bracket that carries the sink is part of the same tolerance stack; see sheet metal brackets .
Tolerances for heat sinks
Full table on the tolerances page .
| Feature | Standard | Achievable with effort | What drives the cost |
|---|---|---|---|
| Base flatness | 0.05 mm | 0.02 mm | Machining allowance, fixture |
| Contact face Ra | Ra 1.6 µm | Ra 0.8 µm; 0.4 by grinding | Extra operations |
| Fin pitch | ±0.10 mm | ±0.05 mm | Process, tool wear |
| Milled features | ±0.02 mm | ±0.01 mm on selective features | Fixture, tool deflection |
Frequently asked questions
- Can you anodise the heat sink but keep the contact face bare? — Yes – the face is masked before anodising. It has to be called out on the drawing; an unmasked anodised face is an insulator and will show up as a hot spot in test.
- Do you supply thermal interface material? — No – the interface is usually specified by the thermal designer. We machine the surface to the flatness and roughness that the material needs.
- What is the tolerance on fin height? — ±0.10 mm as standard for cut fins, ±0.05 mm where the fin height sets the gap to a lid.
- Can you quote a prototype before the die exists? — Yes – machined or bonded prototypes from one piece, then die casting or extrusion once the design is fixed.
Related
- Heat sinks and plates — Extruded, machined and drilled to your interface.
- Application note: heat sink interface — When more fins stop helping and flatness starts to matter.
Send the heat sink drawing with the interface defined
Base flatness, contact finish, mounting method and fin geometry reviewed before the quote goes out.