Die Casting Design: Wall Thickness, Draft and Where the Money Goes
A die casting quote is decided before the die is cut. Wall thickness, draft, parting line and who pays for the tooling move the number far more than the alloy you pick.
1. Wall thickness sets the process
Zinc runs thinner than aluminium – 0.8 mm is possible – but zinc is heavier and the die cost is comparable. Choose by function, not by habit.
| Wall | What it means | Typical use |
|---|---|---|
| 1.0 – 1.5 mm | Thin-wall casting; flow and fill need simulation, porosity risk rises | Small housings, heat spreaders |
| 1.5 – 3 mm | The economical range for aluminium | Enclosures, brackets, motor housings |
| 3 – 4 mm | Heavier sections; sinks and shrinkage need care | Structural parts, mounting bosses |
| Above 4 mm | Shrink porosity is likely; expect machining or a different process | Usually redesigned thinner |
2. Draft, radii and the parting line
The same draft and parting-line rules apply to EMI shielding covers and sheet metal brackets that are cast or stamped.
- Give every face parallel to the die opening 1-2 degrees of draft. Without it the part drags, scuffs and eventually cracks the die.
- Inside corners need a fillet at least equal to the wall thickness; sharp internal corners concentrate stress and shorten die life.
- The parting line leaves a visible witness mark – put it on a face that is not seen or is machined afterwards.
- Ejector pin marks are unavoidable. Place them where they cannot sit on a sealing face or a datum.
3. Where the cost actually sits
| Cost | Driven by | How to keep it down |
|---|---|---|
| Die | Part size, number of slides, surface finish | Fewer undercuts, one parting plane, no polished cosmetic faces unless needed |
| Casting | Shot weight and cycle time | Even walls, generous radii, no isolated thick sections |
| Machining | How many faces need to be cut after casting | Cast the features to near net shape; tolerance only what functions |
| Finishing | Powder coat, anodising, passivation | Mask the mating faces; a fully coated part costs more than a masked one |
4. What to put on the drawing
- Alloy, and whether it is aluminium or zinc
- Wall thickness with a tolerance, and which walls are functional
- Draft angle expectations, or the note “draft as required for casting”
- Machined faces, datums and the tolerance on each
- Cosmetic class – which surfaces are seen, and what defect is acceptable
- Any pressure tightness requirement (for housings holding fluid or gas)
Frequently asked questions
- Is die casting cheaper than CNC machining? — Above a few thousand pieces, usually yes, because the die amortises. Below that, machining a block is normally cheaper and faster, and it lets you test the design before committing to tooling.
- How long does a die take? — Tooling runs in weeks, not days, and the first samples need measurement before production starts. Ask for the die lead time and the first-article lead time separately.
- Can you cast threads? — Threads are normally cut or formed after casting – cast threads are fragile and hard to hold to tolerance. Cast a boss and machine the thread.
- What about porosity? — Some porosity is normal; the question is where. Specify whether the part is cosmetic, structural or pressure tight, and where a void is not acceptable.
Related
- Heat sinks and plates — Cast, extruded or machined – and why mounting fights flatness on a thin base.
- Tolerances by process — What die casting holds, and what a tighter call costs.
More guides on this
- CNC machining: setup count and the price it drives — The companion note for the next decision on the same part.
- Surface finishing: choosing a finish and writing it on the drawing — The companion note for the next decision on the same part.
Send the casting drawing and get the die split out
Die cost, shot cost, machining and finishing as separate lines – within one business day on weekdays.