Case study
Heat sink for a sealed enclosure: fins versus the interface
Adding fins is the obvious answer to a hot component and often the wrong one. In a sealed box the limiting factor is usually the interface between the device and the sink, not the fin area on the outside.
The figures describe the representative case discussed in this note, not a specific customer order.
| Volume | Prototype through serial |
| Material | Extruded or machined aluminium, sealed IP enclosure |
| Route | Machined, drilled and tapped to the interface |
| Control that decides it | Flatness on the mounting face and the interface material before any added fin area |
The situation
A power module sits on a machined aluminium sink inside a sealed IP-rated enclosure. The first build runs hot even though the fin stack matches the thermal model. Measured, the sink’s mounting face is out by 0.15 mm across the footprint, the thermal pad is compressed on one edge only, and the extra fins are radiating into still air inside the box.
What actually moves the temperature
Extruded sinks hold fin geometry cheaply; machined sinks hold flatness and mounting features. Knowing which one is doing the work is the design decision.
| Change | Effect | Cost |
|---|---|---|
| Flatness 0.15 → 0.05 mm on the mounting face | Full pad contact instead of a line | Machining pass; no new tooling |
| More fins inside still air | Little to none | Material and extrusion time |
| Thicker base, thinner fins | Spreads heat to the outer fins | Extrusion profile change |
| Thermal interface material change | Often the largest single gain | Purchased part, no machining |
What we would change in the drawing
- Flatness on the mounting face, with the measurement area stated – not “flat”
- Base thickness and fin thickness as separate dimensions, so the tool can be checked
- Whether the sink is extruded or machined from plate, and the cut length
- Surface treatment: anodising adds a layer; say whether the mounting face must stay bare
Send the sink drawing and the thermal requirement
Heat load, ambient and the interface material – the DFM note comes back with the flatness and finish call on the mounting face.
Frequently asked questions
- What flatness can you hold on a machined mounting face? — 0.05 mm across the mounting area is standard on a machined face; 0.02 mm is achievable with a finishing pass. Extruded faces hold less without machining.
- Does anodising hurt the thermal path? — An anodised layer adds resistance at the interface. If the device mounts directly, leave the mounting face bare or specify a masked area.
- Can you bond or press fins into a base? — Yes, bonded and skived assemblies are quoted where the fin density is beyond what an extrusion profile can hold.
Related
- Heat sinks and plates — The part family this note is about.
- Design guide: heat sink — Fin geometry, flatness and the interface.
Send drawings. Get a reviewed quote.
One business day response, engineering comments included. No account needed.