Case study
Electrical terminal: where contact resistance is decided
A terminal that fits is not a terminal that works. Plating thickness at the contact face, burr on the mating edge and the flatness of a screw pad decide resistance and heat – and all three are cheap to specify before the first batch.
The figures describe the representative case discussed in this note, not a specific customer order.
| Volume | 50,000 per year |
| Material | 0.8 mm C11000 copper, silver 1–5 µm on the contact pad |
| Route | Stamping, two bends, selective plating with masking |
| Control that decides it | Plating thickness and burr limit at the contact face |
The situation
Copper terminal, 0.8 mm C11000, two bends, silver plated only on the contact pad. Volume 50,000 a year. The original drawing said “silver plated” with no thickness and no masking, and the first samples ran hot on a 200 A test.
What the drawing needed
- Plating thickness at the pad – silver 3-5 µm, measured at the contact face, not the average over the part.
- Masking – the two bend lines stay bare so the coating does not crack in the press brake.
- Burr limit – 0.05 mm maximum on the conductor edge; a burr concentrates current and can puncture insulation.
- Contact face roughness – Ra 0.8 µm or better at the pad, which means the die that punches it matters.
- Bend radius – at least 1x thickness, or the copper work-hardens and the spring-back varies batch to batch.
What we measure, and how often
| Check | Method | Frequency |
|---|---|---|
| Plating thickness | XRF at the pad and at a masked edge | Per batch |
| Contact resistance | Four-wire measurement on a sample pair | First article and per batch on request |
| Burr height | Profile projector or microscope | Per batch |
| Dimensional | CMM on hole pattern and bend angle | First article, then per control plan |
Related
- Surface finishing guide — Finish by function, masking cost and how to write it down.
- Terminals and contacts — Plating thickness and contact faces controlled, not assumed.
Send the terminal drawing with the resistance target
Plating, masking and inspection as separate lines – within one business day on weekdays.